1. After the printing, there are bubbles in the UV ink. Additives and unmatched diluents cannot be easily added. If this phenomenon occurs during normal use, please contact the manufacturer for assistance. 2. The viscosity of the screen sticking substrate during printing is too large. Please fill in the matching thinner properly. 3. Check if the print is sticky or not cured after curing Check for circuit problems. 4. Insufficient ink film adhesion after curing Select inks that are suitable for prints. 5. After curing, the ink film is too thick. 6, printing products have a pattern of defects to clean the screen completely, in order to prevent downtime is too long and light curing. 7, the lack of ink film hiding power or too much to adjust the angle of the scraper and the pressure on the screen. 8. Blurred lines when printing small text or fine patterns. 9, appear reticulate. 10. The stencil thinner is too much and the viscosity is too small. Explanation: In addition to the above problems, there are also some problems that are the same as the coating, such as curing problems, adhesion problems, and air bubble problems. The solution refers to the solution of the paint product. (Author: Lucky) Cotton and Linen Table Mat,Rectangular Placemat,Bamboo Placemat Awalong Ceramics Co., Ltd. , http://www.jnceramic.com
Increase the distance between prints and screens.
Increase curing time.
Increase the power of the lamp
Whether the surface of the substrate needs to be processed.
Select the ink that you want to print.
Check the production of the screen for defects.
Replace the scraper with the proper hardness.
Replace the scraper with the proper hardness.
Appropriately fill in the matching diluent to reduce the viscosity.
The mesh is not suitable.